Plaats van herkomst: | Zhejiang, China |
---|---|
Merknaam: | TORICH |
Certificering: | ISO 9001 ISO 14001 TS 16949 |
Modelnummer: | ASTM A790 |
Min. bestelaantal: | 0.5 TON |
Prijs: | negotiable |
Verpakking Details: | Inpakkend op houten, hexagonale doos of andere zeewaardige manieren |
Levertijd: | 15-30 Dagen |
Betalingscondities: | Bevestigingsbrief, D/A, D/P, T/T, Western Union, MoneyGram |
Levering vermogen: | 10000 ton/Jaar |
sleutelwoord:: | Gelaste of Naadloze Roestvrij staalbuizen | Materiaal:: | S31200, S31260, S31500, S31803, S32003, S32101, S32202, S32205 |
---|---|---|---|
Gebruik:: | voor de algemene corrosiedienst | OD:: | 41200mm |
GEWICHT:: | 0.3200m | lengte:: | 112m |
Hoog licht: | roestvast stalen ronde buis,roestvrij buisstaal |
Ferritic of Austenitic Roestvrij staal Gelaste Buizen van ASTM A790 of Naadloze buizen voor de algemene corrosiedienst
Groottewaaier:
O.D.: 4.0230mm W.T.: 130mm L: volgens klantenvereiste
Materiaal en Vervaardiging:
S31200, S31260, S31500, S31803, S32003, S32101, S32202, S32205, S32304, S32506, S32520…
De buizen worden gemaakt van Vlakgewalst staal door automatisch lassenprocédé.
Volgend op lassen en voorafgaand aan definitieve thermische behandeling, zijn de buizen koudgetrokken of koudgewalst
Duplexroestvrij staal:
Het duplexroestvrije staal (DSS), verwijst naar het Ferriet en Austenite elk ongeveer rekenschap gegeven van 50%, over het algemeen minder van het moet ook 30% van roestvrij staal bereiken. Wanneer de Koolstofinhoud laag is, Cr-is de inhoud in 18%~28% en Ni-de inhoud is in 3%~10%. Wat staal bevat etc. ook legeringselementen zoals Mo, Cu, Nb, Ti, N.
Dit die soort staal heeft de kenmerken van Austenite en Ferritic, met ferriet worden vergeleken, heeft het hogere plasticiteit en hardheid, en de de kamertemperatuurbroosheid van nr, intergranular corrosieweerstand en de lassenprestaties zijn beduidend beter. Ondertussen, handhaaft het ook de broosheid 475℃, het hoge warmtegeleidingsvermogen en superplasticity kenmerkend van Ferritic roestvrij staal. Vergeleken met Austenitic roestvrij staal, heeft het met hoge weerstand, en de intergranular corrosieweerstand en corrosie van de chloride de bestand spanning zijn duidelijk beter. Het duplexroestvrije staal heeft uitstekende corrosieweerstand en het is ook een soort nikkel - besparingsroestvrij staal.
Mechanisch Vereiste
Rang: | TP304 | TP304L | TP304LN | TP316 | TP316L | TP316LN | TP316LN | Tpxm-29 | TP304N |
UNS | S30400 | S30403 | S30453 | S31600 | S31603 | S31653 | S31653 | S24000 | S30451 |
Maximum C, | 0,08 | 0,035 | 0,035 | 0,080 | 0,035 | 0,035 | 0,035 | 0,08 | 0,080 |
Maximum Mn, | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 11.5-14.5 | 2.00 |
Maximum P, | 0,045 | 0,045 | 0,045 | 0,045 | 0,045 | 0,045 | 0,045 | 0,060 | 0,045 |
Maximum S, | 0,030 | 0,030 | 0,030 | 0,030 | 0,030 | 0,030 | 0,030 | 0,030 | 0,030 |
Maximum Si, | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 |
Ni | 18.0-20.0 | 18.0-20.0 | 18.0-20.0 | 16.0-18.0 | 16.0-18.0 | 16.0-18.0 | 16.0-18.0 | 17.0-19.0 | 18.0-20.0 |
Cr | 8.0-11.0 | 8.0-13.0 | 8.0-12.0 | 11.0-14.0 | 10.0-14.0 | 11.0-14.0 | 11.0-14.0 | 2.3-3.7 | 8.0-18.0 |
Mo | … | … | … | 2.00-3.00 | 2.00-3.00 | 2.00-3.00 | 2.00-3.00 | … | … |
Stikstof | … | … | … | … | … | … | … | … | … |
Koper | … | … | … | … | … |
Rang: | TP316N | … | … | … | … |
UNS | S31651 | N08367 | N08926 | S31254 | S32654 |
Maximum C, | 0,070 | 0,030 | 0,020 | 0,020 | 0,020 |
Maximum Mn, | 2.00 | 2.00 | 2.00 | 1.00 | 2.0-4.0 |
Maximum P, | 0,045 | 0,040 | 0,030 | 0,030 | 0,030 |
Maximum S, | 0,030 | 0,030 | 0,010 | 0,100 | 0,005 |
Maximum Si, | 4.8-6.0 | 1.00 | 0,50 | 0,80 | 0,50 |
Ni | 9.58.0 | 20.0-22.0 | 24.0-26.0 | 19.5-20.5 | 21.0-23.0 |
Cr | 19.0-22.0 | 23.5-25.5 | 19.0-21.0 | 17.5-18.5 | 24.0-25.0 |
Mo | 0.30-1.50 | 6.0-7.0 | 6.0-7.0 | 6.0-6.5 | 7.0-8.0 |
Stikstof | … | … | … | … | 0.45-0.55 |
Koper | … | … | … | 0.30-0.60 |
Tensilvereisten
Rang en UNS | Treksterkte min ksi [Mpa] |
Opbrengststerkte min ksi [Mpa] |
Verlenging in 2in of 50mm min % |
||||||
304, 316 S30400, S31600 |
75 [515] | 30 [205] | 35 | ||||||
304L, 316L S30403, S31603 |
70 [485] | 25 [175] | 35 | ||||||
Xm-29 S24000 |
100 [690] | 55 [380] | 35 | ||||||
304N, 316N S30451, S31651 |
80 [550] | 35 [240] | 20 | ||||||
304LN, 316LN S30453, S31653 |
75 [515] | 30 [205] | 35 | ||||||
N08367 t≤0.187 | 100 [690] | 45 [310] | 30 | ||||||
N08367 t>0.187 | 95 [655] | 45 [310] | 30 | ||||||
N08926 | 94 [650] | 45 [310] | 35 | ||||||
S31254 t≤0.187 | 100 [690] | 45 [310] | 35 | ||||||
S21254 t>0.187 | 95 [655] | 45 [310] | 35 | ||||||
S32654 | 120 [825] | 65 [450] | 40 |
Toelaatbare Variaties in Afmetingen
Groep | Grootte, Buiten Diameter, in (mm) |
Toelaatbaar Variaties binnen Buiten Diameter, in. [mm] |
Toelaatbaar in GEWICHT, % |
PermisibleVariations in Gesneden Lengte, |
|
1 | Tot 1/2 (12,7), excl. | ±0.005 [0,13] | ±15 | 1/8 [3] | 0 |
2 | 1/2 tot 1 1/2 (12,7 tot 38,1 excl. | ±0.005 [0,13] | ±10 | 1/8 [3] | 0 |
3 | 1 1/2 tot 3 1/2 (38,1 tot 88,9 excl. | ±0.010 [0,25] | ±10 | 3/16 [5] | 0 |
4 | 3 1/2 tot 5 1/2 (88,9 tot 139,7 excl. | ±0.015 [0,38] | ±10 | 3/16 [5] | 0 |
5 | 5 1/2 tot 5 1/2 (139,7 tot 230,2 excl. | ±0.030 [0,76] | ±10 | 3/16 [5] | 0 |
De Lijst van de staalkwaliteitverwijzing
Nr. | China | De V.S. | Japan | Europa | |
Verenigde digitale code | Staal Gade | ASTM A790-05a | JIS G3463.2005 | EN 10217-7.2005 | |
1 | S21953 | 022Cr19Ni5Mo3Si2N | S31500 | - | - |
2 | S22253 | 022Cr22Ni5Mo3N | S31803 | SUS329J3LTB |
X2CrNiMoN22-5-3 1.4462 |
3 | S22053 | 022Cr23Ni5Mo3N | S32205 | - | - |
4 | S23043 | 022Cr23Ni4MoCuN | S32304 | - |
X2CrNiN23-4 1.4362 |
5 | S22553 | 022Cr25Ni6Mo2N | S31200 | - | - |
6 | S22583 | 022Cr25Ni7Mo3WCuN | S31260 | SUS329J4LTB | - |
7 | S25554 | 03Cr25Ni6Mo3Cu2N | S32550 | - | - |
8 | S25073 | 022Cr25Ni7Mo4N | S32750 | - |
X2CrNiMoN25-7-4 1.4410 |
9 | S27603 | 022Cr25Ni7Mo4WCuN | S32760 | - |
X2CrNiMoCuWN25-7-4 1.4501 |
Referentiedocumenten:
ASTM-NORMEN
De Praktijken van ASTM A262 voor het Ontdekken van Gevoeligheid aan Intergranular Aanval in Austenitic Roestvrije stalen
De Specificatie van ASTM A480/van A480 M voor Algemene Eisen ten aanzien van Vlakgewalste Roestvrij en Hitte
Het verzetten vanzich Staal tegen Plaat, Blad en Strook,
De Terminologie van ASTM A941 met betrekking tot Staal, Roestvrij staal, Verwante Legeringen, en Ferrolegeringen.
De Specificatie van ASTM A1016/A1016 M voor Algemene Eisen ten aanzien van Ferritic Legeringsstaal, Austenitic Legering
Staal, en Roestvrij staalbuizen.
De Praktijk van ASTM E527 voor de Nummering van Metalen en Legeringen in het Verenigde Nummeringssysteem (UNS)
De Praktijk van SAE J1086 voor de Nummering van Metalen en Legeringen (UNS)
FAQ
Q: Bent u handelsmaatschappij of fabrikant?
A: Een professionele de materialenuitvinder van staalpijpen, een fabrikant en een oplossingsleverancier
Q: Hoe lang is uw levertijd?
A: Over het algemeen is het 7-14 dagen als de goederen in voorraad zijn. of het is 30-60 dagen als de goederen niet in voorraad zijn, en het is volgens hoeveelheid.
Q: Verstrekt u steekproeven? is het extra vrij of?
A: Ja, konden wij de steekproef voor vrije last aanbieden maar u moet de kosten van vracht betalen.
Q: Wat is uw betalingsvoorwaarden?
A: Payment=1000USD<>, 30% T/T vooraf, saldo vóór verzending.
Als u een andere vraag hebt, pls voel vrij om ons te contacteren